Target: La0.67Ca0.33MnO3compound target
Substrate: STO d290
Pressure: 3 mbar O2
Flow: 40 ml/min
Current: 350 mA
Voltage:379 V
Time: 60 min
Temp: 840 C
Remarks: -
XRR:
Results: 25 nm